Free Standard shipping in the lower 48 on orders of $44 and up

Made in the USA

Made in an ISO 9001:2015 certified facility

Guide

3DRS Resin Settings by Printer

Find starting exposure, burn in and lift settings for 3DRS HERO HD, RPG, Standard HD and Platinum Cure Cast resins on Elegoo, Anycubic, Phrozen, Creality, Uniformation and other resin printers. Search for your printer below, then open its page for settings for every resin colour at 30, 50 and 100 microns, plus Lychee lift, retract and wait values.

Starting values; adjust 0.1 to 0.2 s for your printer and conditions. Questions? Contact us. Last updated November 2, 2026.

Find your printer


Anycubic resin settings

Creality resin settings

Elegoo resin settings

EPAX resin settings

Flashforge resin settings

Nova3D resin settings

Peopoly resin settings

Phrozen resin settings

Prusa resin settings

UniFormation resin settings

How to use these settings

  1. Find your printer and open its page.
  2. Pick the card for your exact resin and colour. Colours cure differently, so each one has its own values.
  3. Enter the normal exposure, burn in layers, burn in exposure and transition layers in Lychee, Chitubox or your printer's slicer.
  4. Enter the lift, retract and wait values from the lift and retract settings.
  5. Print a calibration test and adjust exposure 0.1 to 0.2 s at a time.

Resin settings FAQ

What exposure should I start with for 3DRS resin?

Open your printer below and use the starting value for your resin colour and layer height, then adjust 0.1 to 0.2 s as needed after a calibration print.

Why does each colour have its own settings?

Pigment changes how deeply light cures the resin, so lighter and darker colours of the same resin need different exposure times.

Are there settings for Platinum Cure Cast?

Yes. Every printer page has a Platinum Cure Cast Clear card with exposure, burn in and motion settings, plus print and bake tips. These are starting values based on customer reports and similar clear resin data, so run a test print or exposure test first.

My printer is not listed. What should I do?

Email info@3dresinsolutions.com with your printer and resin and The 3DRS Team will help you find a starting point.

General settings, downloads and post processing

Find starting resin print settings and exposure times for 3DRS HERO HD, RPG and Standard HD resins on Elegoo Saturn, Elegoo Mars, Phrozen Sonic and Anycubic Photon printers in our settings spreadsheet below. This page also lists general lift and speed settings by printer size and our post processing steps. Enter the values in Chitubox, Lychee or your printer's own slicer, then fine tune with a calibration print.

Download the 3DRS Resin Print Settings Spreadsheet

Download the 3DRS resin settings spreadsheet (xlsx) (last updated May 2026)

Calibrate your resin and printer combination

Looking to calibrate? Check out our tutorial on calibrating your resin and printer combo with the 3DRS Starship resin calibration test.

General Resin Printer Settings by Printer Size

General printer Settings Large Format Small to Medium Build Vroom Settings
Bottom Layers 12 8 8
Bottom Exposure Time (s) 35 to 45 s 35 to 45 s 35 to 45 s
Light Off Delay (s) 1 s 1 s 0 s
Bottom Light Off Delay (s) 1 s 1 s 0 s
Bottom Lift Distance (mm) 12 mm 8 mm 8 mm
Lift Distance (mm) 10 mm 7 mm 7 mm
Bottom Lift Speed (mm/min) 40 mm/min 65 mm/min 65 mm/min
Lifting Speed (mm/min) 65 mm/min 100 mm/min 240 mm/min
Retracting Speed (mm/min) 100 mm/min 150 mm/min 240 mm/min

General Post Print Procedures for Resin Prints

Cleaning resin prints with IPA

We recommend post cleaning your prints using clean, high purity 99% IPA (Isopropyl Alcohol). For Best results, utilize Vortex mixers or Ultrasonic Cleaners to quickly remove excess resin for a maximum of 10 to 15 minutes. Avoid leaving prints to soak for extended periods. See Table A for general absorption rates. (Always wear safety glasses and protective gloves when handling 3D Printing Resin).

Post curing resin prints

Completely dry your piece before post curing. Be sure all sides of your print receive equal light exposure to avoid unequal shrinkage on the overexposed side. Unequal cure can damage or dis-form your print. For best results, post cure your print until the surface tack is removed. Extended cure times can increase tensile strength which may be ideal for hollowed prints. When the material is properly post cured, All sides of your print should have equal color and your piece should be noticeably harder.

Table A: IPA and acetone absorption before post curing

Table A: Percent weight gain before post curing "Green Solvent Resistance". 1x1x1 cm cubes printed with Table A settings on Creality LD-002R then immersed in respective solvent for 15 minutes. The lower the absorption rate, the less likely the print will experience surface deformations.

IPA 99% 0 to 0.82 %
Acetone (not recommended) 3.2 %

Share your resin print settings

Please do not hesitate to Contact Us with any questions or comments you may have. If you have the perfect settings on a specific printer you would like us to add, we welcome your input.